How to seam seal a silnylon tent and upgrade the guy lines

This guide shows you how to seal the exposed seams on a silnylon tent and replace the stock guy lines with stronger, adjustable cord. It suits campers doing basic gear repair at home. You need a silicone seam sealant, clean rags and replacement cord.

YouTube video: How to seam seal a tent and upgrade the guy lines featuring the TFS Saga

Caption availability is unknown. Check the CC control in the YouTube player.

Video length
16 min 46 s
Time to do it
2 hours plus overnight cure
Difficulty
Easy
Steps
8

What you need

Steps

  1. Check the tent maker's care info first. Some silnylon tents come factory seam sealed, and sealing a coated seam can make a mess. If sealing is required, work in a ventilated space.

  2. Pitch the tent or set up the fly fully tensioned so the seams are flat and easy to reach. Wipe off dust with a damp cloth and let it dry.

  3. Clean each exposed seam with isopropyl alcohol on a rag. Let it flash off completely. Put on nitrile gloves before handling sealant.

  4. Apply a thin bead of silicone seam sealant along the inside of the stitched seam. Use a small foam brush to push it into the stitch holes.

  5. Work in sections and keep the bead narrow. Wipe away excess before it skins over. Do not seal over zippers or coated fabric beyond the seam.

  6. Leave the tent pitched and fully dry for the cure time on the tube, often 12 to 24 hours. Avoid folding it before the sealant is tack free.

  7. For the guy lines, cut new cord to the length of the old lines plus 30 cm. Melt each cut end with a lighter to stop fraying.

  8. Tie each new line to its guy point with a bowline or lark's head, add a line tensioner, and adjust until the tent pitches taut.

Tips and common mistakes

Test the sealant on a hidden patch of fabric first, because some coatings react badly.

Keep the bead thin; a thick layer takes much longer to cure and can stay tacky.

Work outdoors or in a well-ventilated garage and wear gloves.

Replace one guy line at a time so you can copy the length and attachment point.

Questions

Do I seal the seams on the inside or outside?

Most silnylon tents are sealed on the inside along the exposed stitching. Follow the tent maker's instructions if they specify a different side.

How long before the tent can get wet?

Wait for the full cure time on the sealant tube, usually 12 to 24 hours. Do not pack the tent away while the sealant is still tacky.

Do I need to seam seal a brand new tent?

Only if the manufacturer says sealing is required or the seams leak. Many tents are sold already sealed.